The finish of the cylinder wall decides how well the rings seal and how much oil the wall holds, which affects power, oil consumption and blow-by. Bore preparation is machine-shop work, but an owner planning a build should know what to ask for. This page explains honing and the finish terms. See pistons, connecting rods and rod bolts for the piston side and engine break-in after a rebuild for what happens after assembly.
What honing does
Honing is an abrasive process that improves a bore's geometry and, to a lesser extent, its surface finish. Its main use in engines is finishing the cylinder bores. The bore is honed into a cross-hatch pattern, which holds lubricating oil and helps the piston rings seat and seal (Wikipedia: Honing). If the rings polish the wall too smooth, the cylinder is glazed, which reduces oil retention, interferes with ring seating and can lead to blow-by and wear.
The cross-hatch angle is described in different ways by different sources. One gives a target of about 45 degrees, while builders and ring makers often quote shallower angles. The angle is set by the stone grit, pressure and speed, and a steeper pattern can give poor oil adhesion while a flatter one can hold too much. Do not choose an angle from a general figure: use the ring maker's specification.
Plateau finish and roughness terms
A conventional hone leaves microscopic peaks that can cause blow-by until the rings wear them down, which can take a long time. A plateau finish removes the peaks before assembly, using coarse stones to cut the valleys and finer stones at reduced load to flatten the peaks while keeping the valley depth (EngineLabs Blueprint Series: cylinder honing). The finish is described by:
Rpk, the average peak height, which wears down during break-in.
Rk, the core roughness, the surface that carries most of the ring load.
Rvk, the average valley depth, where oil is held.
Ra, the overall average roughness, which has little useful application for cylinder walls.
Ring makers publish target values by application. As an example, one ring maker's recommendations (in microinches) are Rpk 8 to 12, Rk 30 to 35 and Rvk 40 to 45 for general-purpose street use, Rpk 7 to 10, Rk 18 to 22 and Rvk 28 to 32 for naturally aspirated competition, and Rpk 10 to 15, Rk 35 to 40 and Rvk 50 or more for big-boost, nitrous or supercharged use. Those figures belong to that ring maker and apply to that ring series. Rings that are lapped at the factory are effectively already broken in, so their target peak height can be lower. The hardness of the block matters as well: later blocks and most aftermarket blocks are harder than older ones.
Torque plates
Tightening the cylinder head distorts the bores. A torque plate is a thick plate bolted to the block, with openings for the hone, that recreates that distortion so the bores are honed in the shape they will have when assembled. Some shops circulate hot coolant or oil through the block and plates to simulate thermal distortion as well, which improves the result but adds cost: one shop reports that a heated-oil plate option nearly quadruples the price of honing. Ask whether a torque plate is used, and whether it uses the same fasteners and gasket as the finished engine: head gaskets, head studs and clamp load.
What to ask for
The ring maker's finish specification for the rings and the use, and the piston maker's clearance specification: pistons and rods.
A torque plate, and the head fasteners used with it.
The finish measured and reported, as the parameters above, not only a visual check.
Final sizing for the correct piston-to-wall clearance, as the piston maker specifies.
Thorough cleaning of the bores and block afterwards, following the machinist's and ring maker's instructions, so no abrasive remains.
Bore finish also affects how quickly an engine breaks in and how much blow-by it has: crankcase ventilation, blow-by and oil catch cans.
Sources
Honing (metalworking). Wikipedia. Purpose, cross-hatch, glazing and plateau finish. The article is flagged as needing more citations, and its cross-hatch angle is not relied on. Accessed 2026-11-19.
EngineLabs' Blueprint Series: The Art And Science Of Cylinder Honing. Jeff Smith, EngineLabs, 14 January 2020. Torque plates, plateau parameters and one ring maker's recommendations by use. Accessed 2026-11-19.
Open each version to inspect formatting, tables and photographs.
Revision 1: Cylinder bore preparation and honing
The finish of the cylinder wall decides how well the rings seal and how much oil the wall holds, which affects power, oil consumption and blow-by. Bore preparation is machine-shop work, but an owner planning a build should know what to ask for. This page explains honing and the finish terms. See pistons, connecting rods and rod bolts for the piston side and engine break-in after a rebuild for what happens after assembly.
What honing does
Honing is an abrasive process that improves a bore's geometry and, to a lesser extent, its surface finish. Its main use in engines is finishing the cylinder bores. The bore is honed into a cross-hatch pattern, which holds lubricating oil and helps the piston rings seat and seal (Wikipedia: Honing). If the rings polish the wall too smooth, the cylinder is glazed, which reduces oil retention, interferes with ring seating and can lead to blow-by and wear.
The cross-hatch angle is described in different ways by different sources. One gives a target of about 45 degrees, while builders and ring makers often quote shallower angles. The angle is set by the stone grit, pressure and speed, and a steeper pattern can give poor oil adhesion while a flatter one can hold too much. Do not choose an angle from a general figure: use the ring maker's specification.
Plateau finish and roughness terms
A conventional hone leaves microscopic peaks that can cause blow-by until the rings wear them down, which can take a long time. A plateau finish removes the peaks before assembly, using coarse stones to cut the valleys and finer stones at reduced load to flatten the peaks while keeping the valley depth (EngineLabs Blueprint Series: cylinder honing). The finish is described by:
- Rpk, the average peak height, which wears down during break-in.
- Rk, the core roughness, the surface that carries most of the ring load.
- Rvk, the average valley depth, where oil is held.
- Ra, the overall average roughness, which has little useful application for cylinder walls.
Ring makers publish target values by application. As an example, one ring maker's recommendations (in microinches) are Rpk 8 to 12, Rk 30 to 35 and Rvk 40 to 45 for general-purpose street use, Rpk 7 to 10, Rk 18 to 22 and Rvk 28 to 32 for naturally aspirated competition, and Rpk 10 to 15, Rk 35 to 40 and Rvk 50 or more for big-boost, nitrous or supercharged use. Those figures belong to that ring maker and apply to that ring series. Rings that are lapped at the factory are effectively already broken in, so their target peak height can be lower. The hardness of the block matters as well: later blocks and most aftermarket blocks are harder than older ones.
Torque plates
Tightening the cylinder head distorts the bores. A torque plate is a thick plate bolted to the block, with openings for the hone, that recreates that distortion so the bores are honed in the shape they will have when assembled. Some shops circulate hot coolant or oil through the block and plates to simulate thermal distortion as well, which improves the result but adds cost: one shop reports that a heated-oil plate option nearly quadruples the price of honing. Ask whether a torque plate is used, and whether it uses the same fasteners and gasket as the finished engine: head gaskets, head studs and clamp load.
What to ask for
- The ring maker's finish specification for the rings and the use, and the piston maker's clearance specification: pistons and rods.
- A torque plate, and the head fasteners used with it.
- The finish measured and reported, as the parameters above, not only a visual check.
- Final sizing for the correct piston-to-wall clearance, as the piston maker specifies.
- Thorough cleaning of the bores and block afterwards, following the machinist's and ring maker's instructions, so no abrasive remains.
Bore finish also affects how quickly an engine breaks in and how much blow-by it has: crankcase ventilation, blow-by and oil catch cans.
Sources
Revision 1: Cylinder bore preparation and honing
The finish of the cylinder wall decides how well the rings seal and how much oil the wall holds, which affects power, oil consumption and blow-by. Bore preparation is machine-shop work, but an owner planning a build should know what to ask for. This page explains honing and the finish terms. See pistons, connecting rods and rod bolts for the piston side and engine break-in after a rebuild for what happens after assembly.
What honing does
Honing is an abrasive process that improves a bore's geometry and, to a lesser extent, its surface finish. Its main use in engines is finishing the cylinder bores. The bore is honed into a cross-hatch pattern, which holds lubricating oil and helps the piston rings seat and seal (Wikipedia: Honing). If the rings polish the wall too smooth, the cylinder is glazed, which reduces oil retention, interferes with ring seating and can lead to blow-by and wear.
The cross-hatch angle is described in different ways by different sources. One gives a target of about 45 degrees, while builders and ring makers often quote shallower angles. The angle is set by the stone grit, pressure and speed, and a steeper pattern can give poor oil adhesion while a flatter one can hold too much. Do not choose an angle from a general figure: use the ring maker's specification.
Plateau finish and roughness terms
A conventional hone leaves microscopic peaks that can cause blow-by until the rings wear them down, which can take a long time. A plateau finish removes the peaks before assembly, using coarse stones to cut the valleys and finer stones at reduced load to flatten the peaks while keeping the valley depth (EngineLabs Blueprint Series: cylinder honing). The finish is described by:
- Rpk, the average peak height, which wears down during break-in.
- Rk, the core roughness, the surface that carries most of the ring load.
- Rvk, the average valley depth, where oil is held.
- Ra, the overall average roughness, which has little useful application for cylinder walls.
Ring makers publish target values by application. As an example, one ring maker's recommendations (in microinches) are Rpk 8 to 12, Rk 30 to 35 and Rvk 40 to 45 for general-purpose street use, Rpk 7 to 10, Rk 18 to 22 and Rvk 28 to 32 for naturally aspirated competition, and Rpk 10 to 15, Rk 35 to 40 and Rvk 50 or more for big-boost, nitrous or supercharged use. Those figures belong to that ring maker and apply to that ring series. Rings that are lapped at the factory are effectively already broken in, so their target peak height can be lower. The hardness of the block matters as well: later blocks and most aftermarket blocks are harder than older ones.
Torque plates
Tightening the cylinder head distorts the bores. A torque plate is a thick plate bolted to the block, with openings for the hone, that recreates that distortion so the bores are honed in the shape they will have when assembled. Some shops circulate hot coolant or oil through the block and plates to simulate thermal distortion as well, which improves the result but adds cost: one shop reports that a heated-oil plate option nearly quadruples the price of honing. Ask whether a torque plate is used, and whether it uses the same fasteners and gasket as the finished engine: head gaskets, head studs and clamp load.
What to ask for
- The ring maker's finish specification for the rings and the use, and the piston maker's clearance specification: pistons and rods.
- A torque plate, and the head fasteners used with it.
- The finish measured and reported, as the parameters above, not only a visual check.
- Final sizing for the correct piston-to-wall clearance, as the piston maker specifies.
- Thorough cleaning of the bores and block afterwards, following the machinist's and ring maker's instructions, so no abrasive remains.
Bore finish also affects how quickly an engine breaks in and how much blow-by it has: crankcase ventilation, blow-by and oil catch cans.