The wall has to survive the burn
The substrate is the porous ceramic or metal that the exhaust is forced through. It has to filter at a low pressure drop, survive the temperature of a regeneration, and survive the temperature difference between a channel that is burning and the channel next to it. Those three demands pull in different directions, which is why more than one material is in production. The coating is a separate layer. A bare substrate filters. A washcoat changes the temperature at which the trapped soot will oxidise.
The filter is sized for an application. A material that tolerates a hotter runaway regeneration can be allowed a higher soot mass before the control unit demands a burn. A material that melts sooner has to be regenerated earlier and more carefully. The load model and the regeneration limits belong to that brick, not to a generic DPF.
Cordierite
Cordierite is a magnesium aluminium silicate. It is the usual low-cost automotive substrate. Its thermal expansion is very low, so a one-piece honeycomb survives a temperature gradient better than a material that grows as it heats. It takes a washcoat well, and it is light, so the catalyst on it reaches working temperature quickly.
The limit is the melting point and the conductivity. Heat from a burning channel does not spread sideways quickly. A regeneration that starts with too much soot in one region can melt a hole through the wall, or glaze the pores shut. A melted cordierite brick is scrap. Cleaning will not put the wall back. Passenger-car filters in cordierite are regenerated to a soot limit chosen so that the heat of the burn stays below that damage.
Silicon carbide
Silicon carbide conducts heat much better, and it is mechanically stronger and more resistant to chemical attack. Heat from a local burn spreads, so the peak temperature in one channel is lower for the same soot mass. The expansion when it heats is higher than cordierite. A large one-piece silicon carbide brick cracks from that expansion, so passenger-car filters are built as small segments cemented together with a compliant joint. The joint is part of the filter. A cleaning process that breaks the cement joints has destroyed the brick even if every channel looks clear.
Silicon carbide is the usual choice where the soot load before regeneration is high, or where a runaway burn has to be survived. It costs more than cordierite, and the segmented construction adds pressure drop at the joints.
Aluminium titanate and the less common bodies
Aluminium titanate expands very little and keeps its strength through a thermal shock, so it can be extruded as one monolith rather than a stack of cemented segments. It has been used in light and medium-duty filters for that reason. Acicular mullite is another ceramic used where a high porosity is wanted, so the wall can hold soot and ash with less pressure rise. Metal substrates exist as sintered metal powder, wire mesh, or an alloy foam. They conduct heat well and do not shatter the way a ceramic does, and they are used where that toughness matters more than the cost of the metal.
None of these is identified by looking at the outside of the can. The part number, or a section of a failed brick, is what says which body is fitted. A bake temperature that is safe for silicon carbide can glaze cordierite.
The washcoat
The washcoat is a porous oxide layer fired onto the channel walls. Alumina is the usual carrier. Ceria, zirconia and similar oxides are added as oxygen storage and to keep the alumina from sintering shut. The precious metal, where there is one, is platinum, palladium, or both, dispersed in that layer. Rhodium belongs to a three-way petrol catalyst. A diesel filter is coated for soot with platinum and palladium.
A platinum-bearing coat does two useful things. It oxidises carbon monoxide and hydrocarbons, including the fuel a regeneration has added upstream. It also oxidises nitric oxide to nitrogen dioxide. Nitrogen dioxide attacks soot from about 250 °C, which is a normal exhaust temperature on a loaded run, so a coated filter can lose soot continuously whenever the exhaust is hot enough and there is nitric oxide to convert. That continuous path is passive regeneration. The same platinum raises the nitrogen dioxide leaving the tailpipe, which is why the coat is a compromise and why later systems put a NOx catalyst after the filter.
A heavier platinum loading brings the passive burn down further. A light loading, sometimes used together with a fuel-borne catalyst, is enough to help the additive without making as much nitrogen dioxide. Base-metal coats, without platinum, also lower the oxygen-burn temperature, by less. An uncoated wall needs oxygen and a much hotter exhaust, on the order of 550 to 600 °C, before soot oxidation becomes useful.
The coat lives in the pores. A harsh wash, a thermal clean that sinters the alumina, or oil ash that glasses over the metal, leaves a brick that still filters and no longer lights soot at the temperature the calibration expects. The pressure can look acceptable after a clean while passive regeneration has gone.
How the pieces are combined
| Arrangement | What burns the soot |
|---|---|
| Bare cordierite or silicon carbide | Oxygen, once the control unit has heated the filter into the mid-500s °C or above |
| Washcoat with platinum on the filter, or an oxidation catalyst immediately upstream | Nitrogen dioxide from about 250 °C when the exhaust is lean and hot enough, and oxygen if the control unit forces a hotter burn |
| Fuel-borne catalyst, with or without a light washcoat | The metal from the additive is mixed through the soot, so the oxygen burn starts at a lower temperature. The metal stays behind as ash |
A car can use more than one of these at once. An oxidation catalyst ahead of a coated filter is normal. An additive-assisted filter on a Peugeot or Citroën diesel is the third row, and the additive is specified by generation on the PAT fluid page.